What are the problems often appear when wire galvanized
Often the problem with iron wire galvanized coating roughness, blisters on the coating
Often the problem with iron wire galvanized coating roughness, blisters on the coating, slow deposition rate.
1 rough coatings, passivation film does not shine. Bath temperature is too high; the cathode current density is too large, plating zinc content is too high or sodium hydroxide and DPE content in liquid is too low; the plating solution with solid particles or different metal impurities such as too much will cause this type of failure.
Blister 2 coating, bonding force. Before plating processing not good; bath temperature is too low; additive quality is not good or additives and organic impurities, too much will cause the binding force is not good.
3 slow deposition rate, deep plating ability difference. Low bath temperature; cathodic current density is small; the plating solution of sodium hydroxide content or DPE content is too low, turbid bath or lead different metal impurities will appear this kind of problem.
Tag: